Bisque firing cone: cone 06 or cone 04 before glazing?

Most bisque firings use cone 06 or 04. Learn why bisque stays cooler than the glaze firing, how to choose, and what to log for repeatable results.

By Eutopix Labs P.S.A., the app developer ·

Most potters bisque fire to cone 06 (about 998 °C, 1828 °F) or cone 04 (about 1063 °C, 1945 °F), well below a cone 6 glaze firing. Digitalfire’s reference library lists cone 06 and cone 04 as typical bisque examples.

The bisque has to be hot enough to harden the clay and burn out organic material, but cool enough that it stays porous enough to take glaze. Your clay’s data sheet and your studio’s schedule decide the exact cone.

What a bisque firing is for

A bisque firing turns dry, fragile greenware into a hard, porous ceramic that can be handled and glazed. Digitalfire says the bisque “needs to be low enough to provide sufficient absorbency to make glaze application easy”, and that it also burns off organic material in the clay. The later glaze firing is done at a much higher temperature for stoneware.

Why it matters for your records: a bisque that is too cool leaves more organics in the body, and one that is too hot can reduce how much glaze the piece absorbs. Either can change how a glaze goes on, so the bisque cone belongs in the notes for every piece, not just the glaze firing.

Common bisque and glaze cone pairings

Typical combinations (always confirm with your clay and glaze labels)
Bisque coneOrton °C / °FOften followed by
06998 / 1828A low-fire glaze, or a mid-range glaze fired at cone 5 or 6
041063 / 1945A mid-range glaze at cone 5 or 6 where the studio prefers a firmer bisque
021102 / 2016A higher glaze firing, in the Digitalfire example fired to cone 10 in reduction

Temperatures are from Orton’s chart at 60 °C (108 °F) per hour over the last 100 °C; the pairing column reflects common studio practice and the examples in Digitalfire’s bisque article, not a rule. Some studios fire the same clay to different bisque cones, so use your studio’s standard instead of a general table.

If you rent kiln space, ask which cone and schedule your studio uses for bisque and for glaze, and record both with each piece. If a glaze behaves differently from last time, the difference may be in the bisque rather than in the glaze.

Choosing between 06 and 04

Digitalfire’s bisque article suggests firing as high as the glaze application allows, because a higher bisque can reduce some glaze defects linked to gases leaving the body, as long as the ware stays absorbent enough. Cone 04 gives a firmer, less absorbent piece than cone 06. Cone 06 gives a softer, thirstier piece that takes glaze quickly.

These are practical testing habits, not a substitute for the manufacturer’s instructions.

Problems that trace back to the bisque

When a glaze misbehaves, the bisque is easy to overlook because it happened weeks earlier. Digitalfire’s bisque article links a higher bisque to fewer gas-related glaze defects, because more of the organic material has already burned out of the body. That does not mean a hotter bisque is always better: the same source stresses that the ware must remain absorbent enough for glaze application.

Typical signs worth noting in your journal are a glaze that goes on too thinly or runs off a very absorbent piece, water that pools without soaking in on a very dense piece, and pinholes or blisters after the glaze firing. None of these proves the bisque was the cause, but a note about the bisque cone and how the piece felt during glazing gives you a starting point when you compare two pieces.

A practical habit is to fire a few test tiles in the same bisque as your pieces and keep them for glaze testing. They share the bisque conditions of the work they stand in for, so the test result is relevant.

What to write down for each bisque

That is the same information you need to repeat or avoid the result next time. Our pottery journal guide gives a full list of fields for the piece and the firing.

In Glazeloom you can mark a piece as bisqued, then attach the finished photo after the glaze firing, so the same piece keeps both stages together. You enter the firing details yourself; Glazeloom does not read from a kiln.

Related guides

Frequently asked questions

What cone is bisque fired to?

Common bisque cones are 06 (about 998 °C or 1828 °F) and 04 (about 1063 °C or 1945 °F). Your clay manufacturer or studio may specify a different cone.

Can I glaze fire without a bisque?

Some potters single-fire, applying glaze to greenware or leather-hard clay. It needs a different glazing technique and carries more risk of damage, and your clay and glaze instructions should say whether it is suitable.

Is cone 06 bisque too low for cone 6 clay?

Many potters bisque cone 6 stoneware to 06 or 04. It is a common practice, but follow the clay’s own instructions and check how the glaze applies.

Sources and product details

Keep the next result useful

Glazeloom keeps the choices and observations for each piece together. Download the app to explore its notebook.