Pottery journal template: what to write for every piece and firing

A free pottery journal template: the clay, glaze layer, firing and result fields worth writing down so you can repeat a good piece or avoid a bad one.

By Eutopix Labs P.S.A., the app developer ·

A useful pottery journal records five things for every piece: the clay body, the glazes in the order you applied them, how you applied them, the firing (cone, programme, atmosphere, kiln position) and the result with a photo. Copy the template below into a notebook or note app.

The aim is to be able to find, months later, exactly which combination produced a result you liked.

The template

Print it, copy it into a notebook, or paste it into any notes app. Leave a field blank rather than guess, and write “unknown” when you do not know.

Pottery journal template
SectionWrite down
PieceName or number, date made, form (mug, bowl, test tile), size, photo of the unglazed piece
ClayClay body name, manufacturer, stated cone range, any additions or reclaim
BisqueDate, cone aimed for and cone bent, programme if known, condition afterwards
Glaze layersFor each layer in order: glaze name or code, brand or recipe, number of coats, thickness or dip time, brush, dip or pour
Glaze firingDate, kiln, cone aimed for and cone bent, atmosphere (oxidation or reduction), programme and hold, shelf position
ResultPhoto in consistent light, colour, surface, pooling, crawling or pinholes, what you would change
Next testOne change to try next time and why

Why order and coats matter

Two glazes layered A over B can look different from B over A, and two coats can look different from three. A journal that lists glazes without order or coat counts loses the details that explain the result. Write layers from the bottom up and number them.

Use the full commercial name or code exactly as printed on the jar. Colour names are often reused across brands, and a generic “blue” will not help when you are looking for it a year later.

Photograph the piece from the same side each time, ideally near a window and on a plain background, so colours in different entries can be compared. Add the jar label to the photo set when you can; it saves guessing later whether a glaze was the satin or the gloss version.

Separate what you saw from what you think caused it

Write observations as plain statements: “darker where the two glazes overlap”. Put interpretations in a separate line: “maybe the extra coat did this”. Next time, test the interpretation with one changed variable. Our guide to glaze test tiles shows how to set up that comparison and has a printable record.

A photograph helps but does not settle questions about food safety or suitability for a use. Follow your clay and glaze suppliers’ instructions and your studio’s guidance for those.

Write the next test as a single sentence with one change. A journal that always ends with “next: change X” turns every piece into a small experiment instead of a one-off.

Paper notebook, spreadsheet or app

Any of the three works if you can find a record again. The common failures are not about the format. They are a notebook left at the studio, a phone replaced without a backup, or entries that cannot be searched.

A worked example entry

Here is a fictional entry to show the level of detail that helps. It is an example of format, not a recipe or firing recommendation.

Notice that the entry says what happened and what to change, but it does not say why the pinhole appeared. If you suspect a cause, write it separately and test it.

Ten lines like these take a couple of minutes at the bench and save far more time when you try to repeat a good piece.

Keeping the journal in Glazeloom

Glazeloom is a private pottery notebook for iPhone and iPad. A piece or glaze test holds the clay, ordered glaze layers with application notes, the cone and atmosphere you enter for the firing, photos and flexible notes. You can search by piece, clay or glaze, mark favourites and compare two recorded experiments. It requires no account.

For safety, make a complete backup before changing phones. Glazeloom exports a full backup that includes photos and drafts and can make optional automatic backups to a folder you choose in Files. Restoring adds missing pieces and keeps matching local records. Live syncing between devices is not enabled. The back-up guide explains the steps.

Related guides

Frequently asked questions

What should I write in a pottery journal?

Record the clay body, glaze layers in order with coat counts, application method, the firing (cone, atmosphere, programme, kiln position) and the result with a photo. Add one change to try next.

Do I need an app for a pottery journal?

No. A notebook or spreadsheet works. An app helps with photos, search and comparing two results, provided you can export and back up your records.

How do I make a glaze test tile record?

Label each tile, list the clay, glaze layers and coats, record the firing, and photograph the result. Our test tile guide has a printable record.

Sources and product details

Keep the next result useful

Glazeloom keeps the choices and observations for each piece together. Download the app to explore its notebook.