Cone 04 vs cone 6: which is hotter and when to use each
Cone 6 is about 160 °C hotter than cone 04. See the Orton temperatures side by side and what each cone means for clay, glaze and your firing notes.
Cone 6 is much hotter than cone 04. On the Orton chart at 60 °C (108 °F) per hour, cone 04 is about 1063 °C (1945 °F) and cone 6 is about 1222 °C (2232 °F), a gap of roughly 159 °C (287 °F).
They are also different kinds of firing: cone 04 is a low-fire cone, and cone 6 belongs to the mid-range that Digitalfire describes as where most hobby and studio stonewares and porcelains are fired.
The numbers side by side
| Cone | °F | °C | Relative to cone 6 |
|---|---|---|---|
| 06 | 1828 | 998 | about 224 °C lower |
| 04 | 1945 | 1063 | about 159 °C lower |
| 4 | 2124 | 1162 | about 60 °C lower |
| 5 | 2167 | 1186 | about 36 °C lower |
| 6 | 2232 | 1222 | reference |
| 10 | 2345 | 1285 | about 63 °C higher |
Values are from Orton’s published chart (Fahrenheit) with Celsius converted and rounded; the differences are calculated from those rounded values. Another heating rate shifts every number, so treat the table as a guide to selecting cones rather than a guarantee for your kiln.
Why the zero matters
The cone sequence counts down through zeros before it counts up. Cone 06 is cooler than cone 04, cone 04 is cooler than cone 01, and cone 01 is cooler than cone 1. That is why cone 04 is nowhere near cone 4: on the chart cone 4 is about 99 °C (179 °F) hotter.
A missing zero on a label or in your notes changes the meaning of the whole firing. Write cone numbers exactly as printed, for example “04” and “4”, and avoid shorthand such as “c4”.
What potters use each cone for
Digitalfire’s reference library gives cone 06 and cone 04 as typical bisque firings and calls cone 6 a middle-temperature range where most hobby and studio potters work in electric kilns, with cone 6 the lowest practical range for feldspar-fluxed white plastic bodies. It also notes that cone 6 has the most tested glazes and commercial products.
In practice you will meet cone 04 on low-fire clays and glazes, and cone 6 on stoneware and porcelain. Do not guess from the cone number alone. A clay is designed for a specific cone range and a glaze is formulated to melt at its own. Both the clay and the glaze should be tested at the cone on their labels, and mixing a cone 04 glaze with a cone 6 firing, or the reverse, is a common reason for unexpected results.
- Low-fire glaze fired too hot: it can run off the piece and onto the kiln shelf.
- Mid-range glaze fired too cool: it can look dry, rough or underdeveloped.
- Clay fired below its range: it may stay porous and weak.
Those outcomes are general patterns, not predictions for a particular glaze. Check the manufacturer’s instructions.
What about cone 5 versus cone 6?
Digitalfire describes both as middle temperature, with cone 5 at the low end. The chart puts cone 5 about 36 °C below cone 6 at the same rate. The same source says cone 6 bodies may not fully mature at cone 5 and that many cone 6 glazes still melt well at cone 5, especially with a temperature hold at the end of the firing. A hold changes the heatwork, so write it down.
A worked example of reading two firings
Suppose you have a mug in a cone 04 clay and a bowl in a cone 6 stoneware, and you want to know whether they can share a kiln load. They cannot, at least not without trouble. A firing that brings the bowl to cone 6 will carry the cone 04 mug about 159 °C beyond its intended range, according to the Orton figures above. A firing that suits the mug will leave the bowl at least 159 °C short of cone 6, so its clay and glaze will not mature.
This is the practical reason studios schedule kiln loads by cone. If you rent shelf space, ask the studio which cone each load is aimed at and write it down at the time, not afterwards. Cone numbers on shelves and labels are also easy to misread: a piece marked “04” may be read as “4”, so put the cone in your notes in the same notation as the label.
Write the result of any mismatch you notice, such as a glaze that ran or a clay that stayed soft. Over time those notes form your own reference for what each of your clays and glazes tolerates, which is more reliable for your kiln than a generic chart.
Record the cone with every firing
When a result surprises you, the cone is the first thing to check, and it is the detail people most often forget. Glazeloom has a cone field and an atmosphere field in each firing note, stored with the clay, the ordered glaze layers and your photos. That makes it easy to search your own history for every piece that went to cone 6 and compare two of them side by side. You enter what your studio or kiln provided; the app does not read the kiln.
See the full cone chart in our Orton cone temperature chart, or how to structure the notes in the pottery journal guide.
Related guides
Frequently asked questions
Is cone 6 hotter than cone 04?
Yes. Cone 6 is about 1222 °C (2232 °F) and cone 04 is about 1063 °C (1945 °F) on the Orton chart at 60 °C per hour, roughly 159 °C apart.
Can I fire cone 04 clay to cone 6?
Only if the manufacturer says the clay tolerates it. Low-fire clays are made for lower ranges and can slump or bloat when fired much hotter. Check the product’s data sheet and test first.
Is cone 5 or cone 6 hotter?
Cone 6. On the Orton chart it is about 65 °F (36 °C) higher than cone 5 at the medium heating rate.
Sources and product details