Pottery cone chart: Orton cone temperatures in °C and °F

Orton pyrometric cone temperatures from cone 022 to 14 in Celsius and Fahrenheit, plus how to read a cone chart and why the number is heatwork, not heat.

By Eutopix Labs P.S.A., the app developer ·

Cone 6 is about 1222 °C (2232 °F) and cone 04 is about 1063 °C (1945 °F) on the Orton chart for self-supporting cones heated at 60 °C (108 °F) per hour over the last 180 °F. The full table below runs from cone 022 to cone 14.

A cone number is not a thermometer reading. It is a record of how much heat your ware received, and the temperature next to it changes with how fast the kiln was climbing at the end.

Orton cone temperature chart, cone 022 to 14

The figures below are the Orton Ceramic Foundation’s published values for regular self-supporting cones at the medium heating rate: 108 °F per hour during the last 180 °F of the firing, which is 60 °C per hour for the last 100 °C. The Fahrenheit numbers are copied from Orton’s chart. The Celsius numbers are those Fahrenheit values converted and rounded to the nearest degree.

Orton self-supporting cones at 108 °F (60 °C) per hour
Cone°F°C
0221087586
0211112600
0201159626
0191252678
0181319715
0171360738
0161422772
0151456791
0141485807
0131539837
0121582861
0111607875
0101657903
091688920
081728942
071789976
061828998
05½18591015
0518881031
0419451063
0319871086
0220161102
0120461119
120791137
220881142
321061152
421241162
521671186
5½21971203
622321222
722621239
822801249
923001260
1023451285
1123611294
1223831306
1324281331
1424891365

Cones with a leading zero (06, 04, 022) are cooler than cones without one. Cone 04 at 1945 °F sits well below cone 4 at 2124 °F. The sequence runs 022, 021 … 01, then 1, 2, 3 and upward, so the zero marks the cooler side of cone 1.

Why one cone has several temperatures

Orton publishes the same cone at several heating rates. At 27 °F per hour (slow) cone 6 bends at 2165 °F, at 108 °F per hour it bends at 2232 °F, and at 270 °F per hour (fast) it bends at 2269 °F, according to the same chart. Faster heating needs a higher temperature to produce the same bend.

This is why Orton describes cones as measuring heatwork, the combined effect of time and temperature, rather than temperature alone. A slow, long firing and a fast one can both end with a bent cone 6 while the kiln’s thermocouple shows different peaks.

Orton also states that the chart temperatures were determined in electric kilns in an air atmosphere. Reduction firings can change how some cones behave, and Orton recommends its iron-free cone series for reduction firings between cones 010 and 3.

How to read the cone after the firing

Self-supporting cones are placed on a kiln shelf where you can see them through a spy hole or after opening the kiln. As they absorb heat they bend. The chart’s temperature equivalent applies when the tip has bent over until it is level with the cone’s base. Orton says the difference between a cone at the 4 o’clock position and one touching the shelf is usually only 1 or 2 degrees.

Orton notes that a cone typically takes 15 to 25 minutes to bend once it starts. If the cone you aimed for is still standing, the ware did not reach that heatwork. If it has slumped flat, it went further than planned.

  1. Put a guide cone (one below your target), a firing cone (your target) and a guard cone (one above) on a shelf where you can see them.
  2. After the firing, note which cones bent and how far.
  3. Write the result in your firing notes next to the programme and the position of the cones in the kiln.

Common cone ranges potters mention

Digitalfire’s reference library calls cone 5 and cone 6 “middle temperature” and describes cone 6 as the range where most hobby and studio stonewares and porcelains are fired in electric kilns. Cone 06 and cone 04 are typical bisque cones in the same library’s bisque article. For your own clay and glaze, trust the cone printed on the label, because the manufacturer tested that product at that cone.

If you want to compare two cones in a single line: Orton’s chart puts cone 6 about 65 °F (36 °C) above cone 5 at the medium rate (2232 °F against 2167 °F), and cone 04 more than 280 °F (155 °C) below cone 6. Our comparison of cone 04 and cone 6 goes into the practical difference.

Keep the cone with the piece in Glazeloom

A chart answers “what does this number mean”. It does not remember what you fired, or which glaze came out the way you hoped. In Glazeloom you record the cone and atmosphere you entered for a firing together with the clay body, the ordered glaze layers and photos of the piece, then search by piece, clay or glaze later. Glazeloom does not control a kiln or check temperatures; it keeps your own notes where you can find them.

Glazeloom is a private notebook for iPhone and iPad with no account to create. Our guide to keeping a pottery journal lists the fields worth writing down for each firing.

Related guides

Frequently asked questions

What temperature is cone 6 in Celsius?

On the Orton chart for self-supporting cones heated at 60 °C per hour over the last 100 °C, cone 6 corresponds to about 1222 °C (2232 °F). A slower finish bends the cone at a lower temperature and a faster one at a higher temperature.

Is cone 04 hotter than cone 4?

No. Cone 04 is about 1063 °C (1945 °F) and cone 4 is about 1162 °C (2124 °F) on the same Orton chart. The leading zero means the cone is cooler than cone 1.

Can I trust my kiln controller instead of cones?

A controller reads a thermocouple, which measures temperature. A cone shows how much heatwork the ware received, which is what clay and glaze respond to. Many potters use both and compare them.

Sources and product details

Keep the next result useful

Glazeloom keeps the choices and observations for each piece together. Download the app to explore its notebook.