Cone 5 vs cone 6: temperature gap and how to choose

Cone 6 is about 36 °C (65 °F) hotter than cone 5. See what changes for clay, glazes and kiln wear, and how to log which one you fired.

By Eutopix Labs P.S.A., the app developer ·

On the Orton chart at the medium heating rate, cone 5 is about 1186 °C (2167 °F) and cone 6 is about 1222 °C (2232 °F). Cone 6 is hotter by roughly 36 °C (65 °F). Both are “middle temperature” cones, and many potters and glaze labels treat them as neighbours.

The difference is small on paper but it can matter. A clay needs to be fired to the cone it was designed for to reach its strength, and a glaze may look different one cone higher or lower. The safest rule is to fire to the cone printed on the clay and the glaze, and to write down which one you used.

The two cones side by side

These values are the Orton Ceramic Foundation’s published figures for regular self-supporting cones at 60 °C (108 °F) per hour over the last stretch of the firing. A kiln that climbs faster or slower will reach a given cone at a different temperature, because a cone measures heatwork, not heat alone.

Orton cones 5 and 6 at the medium heating rate
Cone 5Cone 6Difference
°C1186122236
°F2167223265
Often calledLow end of middle temperatureMiddle temperature, common in electric kilns

Our Orton cone chart gives the full range from cone 022 to 14, and the cone 04 vs cone 6 guide explains the difference between a low-fire and a mid-range firing.

What changes with the clay

Digitalfire describes cone 6 as the range where most hobby and studio stonewares and porcelains are fired, and cone 5 as the low end of that range. It also warns that you cannot fire any cone 6 body at cone 5 and expect the same durability. Bodies that are already at their limit are the most affected.

Absorption tests on your own tiles show how dense a clay really is at your cone.

What changes with the glaze

Commercial middle-temperature glazes are often labelled for cone 5 to 6. Digitalfire says most cone 6 glazes still melt well at cone 5, especially with a temperature hold at the end of the firing, and that reactive glazes that are overfired at cone 6 may look better at cone 5.

A glaze can change in several ways between cones: gloss, colour, how far it runs, and how it behaves when layered. Treat any glaze recipe or label as a starting point, and fire a tile at your own kiln’s cone before you commit a whole piece.

Why some potters choose cone 5

Digitalfire lists energy savings and less wear on the elements of an electric kiln. As elements age, a kiln can struggle to climb the last few degrees, and a firing that asks for slightly less temperature is easier on it. It adds that many potters are moving from cone 6 to cone 5 for those reasons.

That is the case for cone 5 if your clay and glazes work there. The case for cone 6 is the opposite: it is the range with the most published glazes, commercial products and recipes, and many clays are specified for it.

How to decide for your own studio

  1. Check the cone range on your clay body label. If it says cone 6, fire at cone 6 unless you test the clay at cone 5.
  2. Check the cone on each glaze. A label “cone 5 to 6” usually means it was tested across both.
  3. Make a tile with the same clay and glaze, fire one at cone 5 and one at cone 6 if your kiln allows it, and compare them side by side.
  4. Note any hold at the end of the firing. A hold adds heatwork, so a cone 5 firing with a long hold can approach cone 6.
  5. If your studio fires the kiln for you, ask which cone and schedule it uses and write that in your notes.

If two firings with the same cone number look different, compare the schedule and the position in the kiln before blaming the glaze.

Where Glazeloom helps, and where it does not

Glazeloom is a private pottery notebook for iPhone and iPad with no account to create. A piece or glaze test stores the clay, the glaze layers in order with coats and application, the cone and atmosphere you enter, photos and notes. A firing note stores the date, kind, cone, atmosphere and schedule, and which pieces were in the kiln. A firing’s detail screen shows the Orton reference temperature for the cone you entered.

Search for 5 or 6 across your own records and compare a cone 5 piece with a cone 6 piece side by side. Glazeloom does not read your kiln, check temperatures or predict how a glaze will fire at a different cone.

Related guides

Frequently asked questions

Is cone 5 or cone 6 hotter?

Cone 6 is hotter. On the Orton chart at 60 °C (108 °F) per hour, cone 6 is about 1222 °C (2232 °F) and cone 5 is about 1186 °C (2167 °F).

Can I fire a cone 6 clay to cone 5?

Sometimes, but the clay may not fully mature. Digitalfire notes that not every cone 6 body reaches the same durability at cone 5, so test absorption and strength on a tile first.

Will cone 6 glazes work at cone 5?

Many do, especially with a hold at the end of the firing, but some change in gloss or colour. Test a tile before using the glaze on finished work.

Does a hold change the cone?

A hold adds heatwork at the top of the firing, so the effective result can be closer to the next cone. Write the hold in your firing notes.

Sources and product details

Keep the next result useful

Glazeloom keeps the choices and observations for each piece together. Download the app to explore its notebook.