Glaze layering combinations: how to test and record them
Test glaze layering combinations on tiles, change one variable at a time, and record layer order, coats and firing so a good overlap can be repeated.
To test glaze layering combinations, make small test tiles from the same clay, apply the glazes in a stated order with a stated number of coats, fire them together, and change only one thing between tiles. Record the layer order, coats and firing for each tile and photograph the result in the same light.
Without those records a pleasing overlap is hard to repeat, because order, thickness and firing can each change the result.
Set up a fair test
Layering results depend on several variables at once: which glaze is on the bottom, how many coats of each, how thick each coat is, the clay underneath and the firing. If you change them all together you will not know which caused the difference.
- Pick two glazes, call them A and B.
- Make or choose test tiles from one clay body, bisqued the same way.
- Number the tiles and photograph them unglazed.
- Apply glazes using one method (brush, dip or pour) and count coats.
- Fire all the tiles in the same firing and, if possible, on the same shelf level.
Our glaze test tile guide includes a printable record for this stage.
A simple test grid
A small grid changes one thing at a time. The example below is a method, not a glaze recipe, and the glazes are placeholders.
| Tile | Bottom layer | Top layer | What changes |
|---|---|---|---|
| 1 | A, 2 coats | none | Control for A |
| 2 | B, 2 coats | none | Control for B |
| 3 | A, 2 coats | B, 2 coats | Order: A under B |
| 4 | B, 2 coats | A, 2 coats | Order: B under A |
| 5 | A, 2 coats | B, 3 coats | Top coat count |
| 6 | A, 3 coats | B, 2 coats | Bottom coat count |
Tiles 1 and 2 show what each glaze does alone on this clay and in this firing. Tiles 3 and 4 isolate order. Tiles 5 and 6 each change one coat count compared with tile 3.
Add a seventh tile with a different clay body only after the grid is done. Clay colour and texture show through thin glaze, so the same layers can look different on white and on speckled clay, and you will want that result recorded separately rather than mixed into the first set.
What to write for every layer
- Exact glaze name or code from the jar, and the brand.
- Position: layer 1 is the first one on the clay.
- Number of coats and how long each dried.
- Application: brushed, dipped or poured, and where the overlap begins.
- Anything unusual: uneven pooling, thin edges, a drip, a wax resist line.
Record the firing separately: cone aimed for and bent, atmosphere, programme and kiln position. Glaze manufacturers publish their own combination suggestions and test conditions; match those conditions before drawing conclusions about your own results. If you are not sure what a number on a cone chart means, our cone chart guide has the Orton temperatures.
If you shorten the notes to save time, keep the three items that most often explain a difference: the layer order, the coat counts and the firing cone.
Describing results so you can compare them later
Use consistent words and a consistent photo set-up. Describe colour, surface (glossy, satin, matte), movement or running, pooling in recesses and any defects such as crawling, pinholes or blistering. Keep “what I saw” apart from “why I think it happened”.
When you make a second round of tiles, start from the best tile in the first round and change one variable again. A short note on every tile, even for bad results, saves you from repeating them. Failed combinations are as useful as the good ones.
Reading the results across the grid
When the tiles come out, lay them in grid order and look at them together. Compare tiles 3 and 4 first: if the order matters, they will differ noticeably. Then compare tile 3 with tiles 5 and 6 to see whether the top or bottom coat count has the bigger effect. Record whether the difference is in colour, surface, movement or all three.
If a tile shows a glaze that has run, check how close it is to the base and to the kiln shelf, and note how thick the application was. Follow your studio’s rules for firing test tiles, because layered glazes can behave differently than either alone.
Keep the tiles. A physical tile is the most reliable reference for colour and surface, and its record tells you how to make it again. Number the back of each tile with the same number as the record.
Finding a combination again in Glazeloom
In Glazeloom a piece or glaze test holds the clay, the glaze layers in order with application notes, the cone and atmosphere you enter for the firing, photos and notes. You can search for a clay or glaze name, mark favourites and compare two recorded experiments, for example tile 3 and tile 4 above. The notebook is private and needs no account.
Glazeloom does not predict how glazes will interact or check safety; it keeps your own observations. Make a backup before you replace your phone; the back-up guide explains how.
Related guides
Frequently asked questions
Does the order of glaze layers matter?
Often yes. The same two glazes can look different with the order reversed, and coat count and thickness also change the result. Test the order with otherwise identical tiles.
How many test tiles do I need for two glazes?
Six covers the basics: each glaze alone, both orders of the pair, and one change of coat count each way. Add more once you know which variable matters.
Can I trust a combination chart from a manufacturer?
Treat it as a starting point. Results depend on the clay, application and firing, so test on your own clay in your own kiln and record the outcome.
Sources and product details
Keep the next result useful
Glazeloom keeps the choices and observations for each piece together. Download the app to explore its notebook.